The sintering and grain growth of natural Indian magnesite as a function of added titania have been studied in the range 0.05 to 0.50 wt% Ti01 with respect to the natural magnesite. Grain sizes in fired compacts have been measured with the aid of an optical microscope on thin and polished sections. The activation energy for grain growth In magnesites with and without added titania has been calculated from the Increase in average grain diameter as a function of firing temperature and time. A higher activation energy of 607 k.J/mol has been observed In the case of natural cryptocrystalline magnesite from Salem with 0.20 to 0.50 wt% titania addition when compared to the activation energy of 293 k.J/mol in natural coarse crystalline magnesite from Almora with 0.50 wt% added titania in the original magnesite. The higher activation energy is attributed to change in the mechanism of sintering due to the addition of titania.
Full text : Subscribe to Download Full Text
[Go Back]
 
MAIN PAGE | SITE MAP | PRIVACY POLICY | TERMS & CONDITIONS  | CONTACT US | FEEDBACK
Copyright Protected 2008, The Indian Ceramic Society. All right reserved.

Developed By : Hi-Tech Soft & Multimedia